Aperture: 95PPI (0.2-10mm); Porosity: 60-98%; Through-hole rate: ≥ 98; Volume density: > 0.1g/cm3 Tensile strength: 8-50MPa; Compressive strength: ≥ 250KPa (compressed to 50% of the pressure value); Mechanical strength: 2-7MPa; High temperature: > 300 ℃; Heat transfer coefficient: > 3w/(m2k) Application: As the electrode material of alkaline rechargeable battery, it is the most promising electrode material for battery manufacturers to replace foam nickel and reduce production costs.
Aperture 95PPI (0.2-10mm); Porosity 60-98%; Through-hole rate ≥ 98; Volume density > 0.1g/cm3
Tensile strength 8-50MPa; Compressive strength ≥ 250KPa (compressed to 50% of the pressure value); Mechanical strength 2-7MPa; High temperature > 300 ℃; Heat transfer coefficient > 3w/(m2k)
Application As the electrode material of alkaline rechargeable battery, it is the most promising electrode material for battery manufacturers to replace foam nickel and reduce production costs.